一般大气环境下锈蚀结构钢表面特征与随机模型
王友德1,2(),徐善华1,2,李晗1,2,张海江1,2
Surface Characteristics and Stochastic Model of Corroded Structural Steel Under General Atmospheric Environment
WANG Youde1,2(),XU Shanhua1,2,LI Han1,2,ZHANG Haijiang1,2

图12. 锈坑深度与锈坑形状的关系

Fig.12. Relationship between pit depth and pitting shape parameter (hmax—maximum depth of pits; ha', hb', hc'—relative depths of pits)