一般大气环境下锈蚀结构钢表面特征与随机模型
王友德1,2(),徐善华1,2,李晗1,2,张海江1,2
Surface Characteristics and Stochastic Model of Corroded Structural Steel Under General Atmospheric Environment
WANG Youde1,2(),XU Shanhua1,2,LI Han1,2,ZHANG Haijiang1,2

图10. 锈坑深度对数均值(μh)和锈坑径深化对数均值(μAr)变化规律

Fig.10. Changing laws of μh (a) and μAr (b)