一般大气环境下锈蚀结构钢表面特征与随机模型
|
|
王友德,徐善华,李晗,张海江
|
Surface Characteristics and Stochastic Model of Corroded Structural Steel Under General Atmospheric Environment
|
|
Youde WANG,Shanhua XU,Han LI,Haijiang ZHANG
|
|
| 表3 锈坑特征参数统计结果 |
| Table 3 Characteristic parameters of corrosion pits of steel plates |
|
Sample No. | Pd / cm-2 | μh | σh | μ | σ |
|---|
| Side A | Side B | Side A | Side B | Side A | Side B | Side A | Side B | Side A | Side B |
|---|
| A1 | 22.2 | 19.1 | 4.91 | 5.09 | 0.19 | 0.16 | 1.58 | 1.55 | 0.55 | 0.53 | | A2 | 20.5 | 20.1 | 5.21 | 5.35 | 0.20 | 0.18 | 1.56 | 1.62 | 0.69 | 0.63 | | A3 | 19.4 | 18.5 | 5.68 | 5.51 | 0.07 | 0.10 | 0.90 | 1.43 | 0.61 | 0.59 | | A4 | 16.2 | 17.2 | 5.75 | 5.80 | 0.11 | 0.21 | 0.94 | 0.85 | 0.60 | 0.63 | | A5 | 12.5 | 13.2 | 5.63 | 5.82 | 0.13 | 0.14 | 1.21 | 0.92 | 0.64 | 0.66 | | A6 | 10.1 | 11.5 | 5.88 | 5.95 | 0.24 | 0.16 | 1.33 | 0.95 | 0.63 | 0.60 | | HTF | 20.2 | 6.4 | 5.46 | 6.47 | 0.53 | 0.38 | 0.97 | 0.34 | 0.69 | 0.69 | | HBF | 6.9 | 7.5 | 6.38 | 6.23 | 0.39 | 0.31 | 0.72 | 0.72 | 0.54 | 0.68 | | HW | 9.4 | 11.5 | 6.34 | 5.98 | 0.34 | 0.21 | 0.16 | 0.25 | 0.5 | 0.53 | | STF | 15.7 | 7.6 | 5.40 | 6.35 | 0.40 | 0.44 | 1.24 | 0.61 | 0.64 | 0.66 | | SBF | 13.4 | 10.7 | 5.88 | 5.72 | 0.67 | 0.48 | 0.43 | 0.57 | 0.62 | 0.60 | | SW | 8.6 | 6.8 | 5.89 | 6.46 | 0.38 | 0.36 | 1.07 | 0.68 | 0.51 | 0.51 | | VTF | 15.3 | 14.6 | 5.49 | 5.80 | 0.47 | 0.63 | 0.58 | 0.24 | 0.49 | 0.62 | | VBF | 11.0 | 13.3 | 6.09 | 6.27 | 0.50 | 0.34 | 0.28 | 0.24 | 0.56 | 0.56 | | VW | 12.2 | 14.5 | 5.91 | 5.70 | 0.35 | 0.39 | 0.69 | 0.73 | 0.49 | 0.59 |
|
|
|