| 表2 锈蚀深度参数统计结果 |
| Table 2 Corrosion depth parameters of steel plates |
|
Sample No. | Δtave / μm | tsd / μm | κ1 | κ2 |
|---|
| Side A | Side B | Side A | Side B | Side A | Side B | Side A | Side B |
|---|
| A1 | 117 | 82 | 36 | 28 | 1.02 | 0.92 | 0.45 | 0.42 | | A2 | 173 | 134 | 58 | 46 | 0.98 | 1.05 | 0.50 | 0.46 | | A3 | 208 | 167 | 58 | 62 | 1.03 | 1.12 | 0.45 | 0.45 | | A4 | 243 | 245 | 64 | 78 | 1.24 | 1.28 | 0.60 | 0.58 | | A5 | 242 | 241 | 60 | 80 | 1.22 | 1.15 | 0.64 | 0.59 | | A6 | 267 | 257 | 94 | 87 | 1.39 | 1.48 | 0.75 | 0.70 | | HTF | 310 | 576 | 138 | 186 | 2.47 | 2.48 | 0.95 | 1.06 | | HBF | 397 | 500 | 164 | 177 | 2.34 | 2.28 | 0.97 | 1.10 | | HW | 291 | 433 | 115 | 146 | 1.98 | 2.18 | 0.98 | 0.96 | | STF | 284 | 533 | 156 | 180 | 2.79 | 2.50 | 0.89 | 1.02 | | SBF | 340 | 498 | 157 | 167 | 2.08 | 2.15 | 1.13 | 1.15 | | SW | 382 | 532 | 173 | 178 | 2.29 | 2.26 | 0.68 | 1.13 | | VTF | 281 | 434 | 145 | 110 | 1.31 | 2.03 | 0.52 | 1.02 | | VBF | 320 | 467 | 138 | 163 | 2.17 | 2.44 | 0.95 | 1.06 | | VW | 397 | 207 | 164 | 90 | 2.24 | 1.52 | 0.97 | 0.56 |
|
|
|