X80钢焊接接头在模拟天然气凝析液中的腐蚀行为
陈芳,李亚东,杨剑,唐晓,李焰

Corrosion Behavior of X80 Steel Welded Joint in Simulated Natural Gas Condensate Solutions
Fang CHEN,Yadong LI,Jian YANG,Xiao TANG,Yan LI
表3 模拟天然气凝析液中X80钢BM和WM在不同温度中的EIS拟合数据
Table 3 Fitting data of EIS of BM and WM in simulated natural gas condensate at different temperatures

Specimen

T

℃

Rs

Ω·cm2

Cdl

μF·cm-2

n

Rp

Ω·cm2

RL

Ω·cm2

L

H·cm-2

BM303.15200.84135.0292.0312.4
402.76920.8578.7234.1121.3
502.812200.8424.662.714.1
602.732100.7811.623.62.1
WM304.41640.85304.2
403.82150.84151.4--
503.23090.82110.0--
603.04400.8359.0--