X80钢焊接接头在模拟天然气凝析液中的腐蚀行为
陈芳,李亚东,杨剑,唐晓,李焰()
Corrosion Behavior of X80 Steel Welded Joint in Simulated Natural Gas Condensate Solutions
CHEN Fang,LI Yadong,YANG Jian,TANG Xiao,LI Yan()

图7. 模拟天然气凝析液中X80钢BM和WM在不同HAc浓度溶液中的EIS

Fig.7. EIS of BM (a) and WM (b) in simulated natural gas condensate in different concentrations of HAc