[an error occurred while processing this directive]
X80钢焊接接头在模拟天然气凝析液中的腐蚀行为
陈芳,李亚东,杨剑,唐晓,李焰()
Corrosion Behavior of X80 Steel Welded Joint in Simulated Natural Gas Condensate Solutions
CHEN Fang,LI Yadong,YANG Jian,TANG Xiao,LI Yan()

图4. EIS等效电路图

Fig.4. Equivalent circuit for fitting EIS data (Rs—solution resistance, Rp—polarization resistance, RL—inductive resistance, L—inductance, Cdl—double layer capacitance)