[an error occurred while processing this directive]
NM500耐磨钢拉伸过程中TiN的破碎机制
吴翔,左秀荣(),赵威威,王中洋
Mechanism of TiN Fracture During the Tensile Process of NM500 Wear-Resistant Steel
WU Xiang,ZUO Xiurong(),ZHAO Weiwei,WANG Zhongyang

图9. NM500钢在厚度1/4和厚度中心的质量图及取向差定量分析

Fig.9. The image quality (IQ) maps of microstructure types of a quarter of thickness (a) and center of thickness (b), and quantitative analysis of distribution of misorientation angle of grains in a quarter of thickness and center of thickness (c) (θ means the angle of boundary, black line 15°≤θ≤50°, red line θ>50°)