NM500耐磨钢拉伸过程中TiN的破碎机制
吴翔,左秀荣(),赵威威,王中洋
Mechanism of TiN Fracture During the Tensile Process of NM500 Wear-Resistant Steel
WU Xiang,ZUO Xiurong(),ZHAO Weiwei,WANG Zhongyang

图6. 热力学平衡状态下NM500钢中各相的质量分数及温度与奥氏体中Ti含量的关系

Fig.6. Mass fraction of phases as a function of temperature in NM500 steel at thermodynamic equilibrium state (a) and the relationship between temperature and Ti content in austenite (b)