Ti70-xTa15Zr15Fex (x=0.3、0.6、1.0)形状记忆合金薄膜的马氏体相变与阻尼行为
|
|
Martensitic Transformation and Damping Behavior of Ti70-xTa15Zr15Fex (x=0.3, 0.6, 1.0) Shape Memory Thin Films
|
|
图5. Ti70-xTa15Zr15Fex (x=0.3、0.6、1.0)合金薄膜室温下的拉伸应力-应变曲线 |
Fig.5. Tensile stress-strain curves of Ti70-xTa15Zr15Fex (x=0.3, 0.6, 1.0) thin films |
![]() |