Ti70-xTa15Zr15Fex (x=0.3、0.6、1.0)形状记忆合金薄膜的马氏体相变与阻尼行为
|
|
Martensitic Transformation and Damping Behavior of Ti70-xTa15Zr15Fex (x=0.3, 0.6, 1.0) Shape Memory Thin Films
|
|
图3. Ti70-xTa15Zr15Fex (x=0.3、0.6、1.0)合金薄膜的粒径分布图 |
Fig.3. Grain size distributions of Ti70-xTa15Zr15Fex thin films with x=0.3 (a), 0.6 (b) and 1.0 (c) |
![]() |