微生物抑制5754铝合金的海水腐蚀行为
|
|
Corrosion Inhibition Effect of Microorganism on 5754 Al Alloy in Seawater
|
|
图4. 5754铝合金在不含微生物B.subtilis的海水中浸泡不同时间的EIS |
Fig.4. EIS of the 5754 Al alloy in seawater without B.subtilis for different immersion time (Z'—real part of impedance, Z''—imaginary part of impedance, Z—impedance, f—frequency) |
![]() |