微生物抑制5754铝合金的海水腐蚀行为
|
|
Corrosion Inhibition Effect of Microorganism on 5754 Al Alloy in Seawater
|
|
图3. 5754铝合金浸泡前后的表面腐蚀轮廓图 |
Fig.3. 2D (a, c, e) and 3D (b, d, f) surface profile images of 5754 Al alloy before (a, b), and after immersion for 15 d in sterile (c, d) and inoculated B.subtilis (e, f) seawater (Arrows show the locations of pitting) |
![]() |