[an error occurred while processing this directive]
CMT增材制造TC4-DT合金组织均匀性与力学性能一致性研究
杜子杰1,2, 李文渊2(), 刘建荣2, 锁红波3, 王清江2
Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process
DU Zijie1,2, LI Wenyuan2(), LIU Jianrong2, SUO Hongbo3, WANG Qingjiang2

图14. CMT成形TC4-DT试块不同区域的滑移程示意图

Fig.14. The schematics of slip length of overlapping zone (a), top of the ordinary deposition zone (b) and bottom of the ordinary deposition zone (c) of the TC4-DT sample deposited by CMT