CMT增材制造TC4-DT合金组织均匀性与力学性能一致性研究
杜子杰1,2, 李文渊2(), 刘建荣2, 锁红波3, 王清江2
Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process
DU Zijie1,2, LI Wenyuan2(), LIU Jianrong2, SUO Hongbo3, WANG Qingjiang2

图11. D试样在1%塑性变形后不同选区的滑移形貌、EBSD取向图及转变α相反极图
Color online
(a~c) overlapping lines(d~f) 1st area on the ordinary deposition zone(g~i) 2nd area on the ordinary deposition zone

Fig.11. Slip characteristics (a, d, g), the relative EBSD maps (b, e, h) and IPF-X (c, f, i) for transformed α phase of different areas on sample D after 1% plastic deformation (μ—Schmid factor)