CMT增材制造TC4-DT合金组织均匀性与力学性能一致性研究
杜子杰1,2, 李文渊2(), 刘建荣2, 锁红波3, 王清江2
Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process
DU Zijie1,2, LI Wenyuan2(), LIU Jianrong2, SUO Hongbo3, WANG Qingjiang2

图9. 不同取样位置试样断口侧面形貌

Fig.9. Macrostructures (a, c, e) and SEM images of fracture side (b, d, f) of samples D (a, b), 1# (c, d) and 2# (e, f)