CMT增材制造TC4-DT合金组织均匀性与力学性能一致性研究
杜子杰1,2, 李文渊2(), 刘建荣2, 锁红波3, 王清江2
Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process
DU Zijie1,2, LI Wenyuan2(), LIU Jianrong2, SUO Hongbo3, WANG Qingjiang2

图5. CMT成形TC4-DT合金试块搭接区高倍组织
(a, b) overlapping zone with different magnifications(c, d) microstructures above (c) and below (d) the overlapping line

Fig.5. Microstructures of the overlapping zone of the TC4-DT sample deposited by CMT