[an error occurred while processing this directive]
CMT增材制造TC4-DT合金组织均匀性与力学性能一致性研究
杜子杰1,2, 李文渊2(), 刘建荣2, 锁红波3, 王清江2
Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process
DU Zijie1,2, LI Wenyuan2(), LIU Jianrong2, SUO Hongbo3, WANG Qingjiang2

图2. 室温拉伸实验板状拉伸试样、取样位置及拉伸变形行为研究观察选区

Fig.2. The schematic of tensile sample (unit: mm) (a), sampling position (b) and the observation areas of D sample after 1% plastic deformation (c) (D: overlapping zone; 1#: top of the ordinary deposition zone; 2#: bottom of the ordinary deposition zone)