气孔与晶界相互作用的相场模拟
孙正阳, 王昱天, 柳文波

Phase-Field Simulation of the Interaction Between Pore and Grain Boundary
SUN Zhengyang, WANG Yutian, LIU Wenbo
表2 不同气孔率下的晶粒生长指数
Table 2 Grain growth exponents at different fp
fpnR2
02.050.990
2%2.440.997
4%3.150.992
8%4.190.995