气孔与晶界相互作用的相场模拟
|
|
Phase-Field Simulation of the Interaction Between Pore and Grain Boundary
|
|
图4. 不同梯度参数κc下相场变量的平衡取值 |
Fig.4. Equilibrium profiles for phase field variables at different κc(a) orientation field variables η |
![]() |