气孔与晶界相互作用的相场模拟
|
|
Phase-Field Simulation of the Interaction Between Pore and Grain Boundary
|
|
图2. 不同梯度参数κα下取向场变量η |
Fig.2. Equilibrium profiles for phase field variables at different κα(a) orientation field variables η |
![]() |