基于恒过热控制的感应加热中间包内钢水的流动与传热
唐海燕(), 李小松, 张硕, 张家泉
Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control
TANG Haiyan(), LI Xiaosong, ZHANG Shuo, ZHANG Jiaquan

图15. 1000 kW加热功率下A0和A4方案不同时刻水口中心截面速度矢量图
Color online
(a1, a2) 200 s (b1, b2) 500 s (c1, c2) 1500 s (d1, d2) 3000 s

Fig.15. Velocity vector diagrams on longitudinal section of outlet centre at different moments for cases A0 (a1~d1) and A4 (a2~d2) with 1000 kW heating power