基于恒过热控制的感应加热中间包内钢水的流动与传热
|
|
Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control
|
|
图14. 1000 kW加热功率下A0和A4方案不同时刻通道纵截面速度矢量图 |
Fig.14. Velocity vector diagrams along channel longitudinal section at different moments for cases A0 (a1~d1) and A4 (a2~d2) with 1000 kW heating power (Ellipses in Fig.14d1 represent circulating flows) |
![]() |