Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control
TANG Haiyan(), LI Xiaosong, ZHANG Shuo, ZHANG Jiaquan

图13. 开启及未开启感应加热中间包水口纵截面温度场
Color online
(a) without induction heating (b) with induction heating (1000 kW, 3000 s)

Fig.13. Temperature fields of the outlet longitudinal section