基于恒过热控制的感应加热中间包内钢水的流动与传热
唐海燕(), 李小松, 张硕, 张家泉
Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control
TANG Haiyan(), LI Xiaosong, ZHANG Shuo, ZHANG Jiaquan

图12. 1000 kW加热功率下加热不同时间时X2截面温度场
Color online
(a) 200 s (b) 500 s (c) 1500 s (d) 3000 s

Fig.12. Temperature fields in X2 section at different moments with 1000 kW heating power