基于恒过热控制的感应加热中间包内钢水的流动与传热
唐海燕(), 李小松, 张硕, 张家泉
Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control
TANG Haiyan(), LI Xiaosong, ZHANG Shuo, ZHANG Jiaquan

图7. 中间包感应加热通道内电磁力分布
Color online

Fig.7. Electromagnetic force (Fmag) distribution in the induction heating channels