基于恒过热控制的感应加热中间包内钢水的流动与传热
|
Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control
|
图4. A4方案数值模拟与水模拟实验[ |
Fig.4. Comparisons of residence time distribution (RTD) curves between numerical (a) and water modelling[ |
![]() |