基于非对称双悬臂梁模型优化的双金属板界面结合强度研究
秦勤1,2(), 李程2, 何流1, 叶陈龙2, 臧勇1
An Investigation of Interface Bonding Strength of Bimetal Plate Based on the Optimization of Asymmetric Double Cantilever Beam Model
QIN Qin1,2(), LI Cheng2, HE Liu1, YE Chenlong2, ZANG Yong1

图11. 不同压下量下圆锥制件的截面轮廓和底部鼓包高度

Fig.11. Sectional profiles of conical parts under different reductions (a) and the heights of bulge defect under different reductions (b)