基于非对称双悬臂梁模型优化的双金属板界面结合强度研究
|
An Investigation of Interface Bonding Strength of Bimetal Plate Based on the Optimization of Asymmetric Double Cantilever Beam Model
|
图9. 单点渐进成形仿真结果与实验结果的对比 |
Fig.9. Comparisons between the result of single point incremental forming |
![]() |