基于非对称双悬臂梁模型优化的双金属板界面结合强度研究
|
An Investigation of Interface Bonding Strength of Bimetal Plate Based on the Optimization of Asymmetric Double Cantilever Beam Model
|
图8. 复合板损伤模拟结果 |
Fig.8. Simulated result of the bimetal sheet damage |
![]() |