卷取温度对500 MPa级热冲压桥壳用钢组织与力学性能的影响
惠亚军1,2(), 刘锟1, 吴科敏3, 李秋寒1, 牛涛4, 武巧玲4
Effect of Coiling Temperature on Microstructure and Mechanical Properties of 500 MPa Grade Hot Stamping Axle Housing Steel
HUI Yajun1,2(), LIU Kun1, WU Kemin3, LI Qiuhan1, NIU Tao4, WU Qiaoling4

图5. 500 MPa级热冲压桥壳用钢中析出物的TEM像和EDS分析

Fig.5. TEM images (a, c) and EDS analyses (b, d) of precipitates (showed by arrows) in 500 MPa grade hot stamping axle housing steel when coiling at 600 ℃ (a, b) and 570 ℃ (c, d)