卷取温度对500 MPa级热冲压桥壳用钢组织与力学性能的影响
|
Effect of Coiling Temperature on Microstructure and Mechanical Properties of 500 MPa Grade Hot Stamping Axle Housing Steel
|
图3. 500 MPa级热冲压桥壳用钢在570 ℃卷取时的EBSD结果 |
Fig.3. EBSD results of 500 MPa grade hot stamping axle housing steel when coiling at 570 ℃ |
![]() |