基于原位TEM拉伸的稀土H13钢塑性形变行为和断裂机制
|
|
Plastic Deformation Behavior and Fracture Mechanism of Rare Earth H13 Steel Based on In Situ TEM Tensile Study
|
|
图4. 稀土H13钢原位拉伸试样裂纹形貌的TEM像 |
Fig.4. TEM images showing crack morphologies of in situ tensile specimen of rare earth H13 steel (TD—tensile direction, FD—fracture direction) |
![]() |