热轧变形量对高钛耐磨钢组织与力学性能的影响
许帅, 孙新军, 梁小凯, 刘俊, 雍岐龙

Effect of Hot Rolling Deformation on Microstructure and Mechanical Properties of a High-Ti Wear-Resistant Steel
XU Shuai, SUN Xinjun, LIANG Xiaokai, LIU Jun, YONG Qilong
表1 不同轧制变形量高钛耐磨钢轧制工艺
Table 1 Rolling process of high Ti wear-resistant steel with different rolling deformations
Sample No.The actual thickness of the plate after each pass / mmTotal reduction ratio
90-3090-72-58-(950 ℃)-44-35-(850 ℃)-303∶1
90-1890-72-58-(950 ℃)-44-33-(850 ℃)-24-185∶1
90-1290-72-58-(950 ℃)-44-33-24-18-(850 ℃)-14-127.5∶1
90-990-72-58-(950 ℃)-44-33-24-18-(850 ℃)-13-910∶1
90-390-72-58-(950 ℃)-44-33-24-18-13-9-(850 ℃)-6-4-330∶1