热轧变形量对高钛耐磨钢组织与力学性能的影响
许帅1, 孙新军1(), 梁小凯1, 刘俊2, 雍岐龙1
Effect of Hot Rolling Deformation on Microstructure and Mechanical Properties of a High-Ti Wear-Resistant Steel
XU Shuai1, SUN Xinjun1(), LIANG Xiaokai1, LIU Jun2, YONG Qilong1

图10. No.90-18样品冲击断口处TiC粒子的SEM像和EDS结果

Fig.10. SEM image (a) and EDS result (b) of TiC particle in fracture morphology