热轧变形量对高钛耐磨钢组织与力学性能的影响
|
Effect of Hot Rolling Deformation on Microstructure and Mechanical Properties of a High-Ti Wear-Resistant Steel
|
图7. 不同轧制工艺高钛耐磨钢中的TiC粒径分布图 |
Fig.7. TiC particle diameter distribution of high-Ti wear- resistant steel with different rolling processes |
![]() |