热轧变形量对高钛耐磨钢组织与力学性能的影响
|
Effect of Hot Rolling Deformation on Microstructure and Mechanical Properties of a High-Ti Wear-Resistant Steel
|
图5. TiC析出相的TEM像、HRTEM像、SAED花样和EDS结果 |
Fig.5. TEM images of TiC precipitate in samples No.90-30 (a), No.90-12 (b) and No.90-3 (c), and HRTEM image (d), SAED pattern (e) and EDS result (f) of TiC particle in sample No.90-12 (d(111)—interplanar spacing of (111)) |
![]() |