热轧变形量对高钛耐磨钢组织与力学性能的影响
许帅1, 孙新军1(), 梁小凯1, 刘俊2, 雍岐龙1
Effect of Hot Rolling Deformation on Microstructure and Mechanical Properties of a High-Ti Wear-Resistant Steel
XU Shuai1, SUN Xinjun1(), LIANG Xiaokai1, LIU Jun2, YONG Qilong1

图3. 不同轧制工艺高钛耐磨钢原奥氏体晶粒的OM像

Fig.3. OM images of prior-austenite microstructures in high-Ti wear-resistant steel samples No.90-30 (a), No.90-18 (b), No.90-12 (c), No.90-9 (d) and No.90-3 (e)