形变及退火工艺对Fe47Mn30Co10Cr10B3双相高熵合金组织演变的影响
刘怡, 涂坚, 杨威华, 尹瑞森, 谭力, 黄灿, 周志明

Effect of Deformation and Annealing Treatment on Microstructure Evolution of Fe47Mn30Co10Cr10B3 Dual-Phase High-Entropy Alloy
LIU Yi, TU Jian, YANG Weihua, YIN Ruisen, TAN Li, HUANG Can, ZHOU Zhiming
表1 图2c中第二相颗粒及基体的EDS分析结果 (atomic fraction / %)
Table 1 EDS results of the second phase particles and the matrix phase in Fig.2c
LocationFeMnCoCrB
117.4424.461.3447.918.85
247.0627.349.8010.625.18