[an error occurred while processing this directive]
铁基非晶合金局域结构与性能关联:基于微合金化机理研究
耿遥祥1(), 王英敏2
Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research
GENG Yaoxiang1(), WANG Yingmin2

图5. 直径(D)为1 mm的[Si-B2Fe8]Fe和[Si-B2Fe7.6RE0.4]Fe样品及非晶形成临界直径(Dc)样品[Si-B2Fe7.6ETM0.4]Fe的XRD谱

Fig.5. XRD spectra of the [Si-B2Fe8]Fe and [Si-B2Fe7.6RE0.4]Fe rod samples with diameter (D) of 1.0 mm (a), and the [Si-B2Fe7.6ETM0.4]Fe alloys with critical diameter for glass formation (Dc) (b)