[an error occurred while processing this directive]
铁基非晶合金局域结构与性能关联:基于微合金化机理研究
耿遥祥1(), 王英敏2
Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research
GENG Yaoxiang1(), WANG Yingmin2

图3. 不同元素之间的混合焓及各自的原子半径

Fig.3. The equal-atomic ratio enthalpy of mixing (ΔH, kJ/mol) data of B, Si (a) and Fe (b) with the early transition metals (ETMs, Zr, Hf, Nb and Ta) and rare earth elements (RE, Y, Ce, Pr, Nd, Sm, Gd and Dy) (The Goldschmidt radii (nm) of these elements are also presented)
Color online