Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research
|
|
图2. 非晶合金中团簇内部和团簇间原子关联作用及合金化原子在模型结构中的位置示意图 |
Fig.2. Schematics of the intra- and inter-cluster correlations in the amorphous structures and the position of alloying atoms entering the model structure (C stand for the center atoms, S stand for the shell atoms, G stand for the glue atoms, A stand for the alloying atoms, subscripts 1 and 2 stand for their corresponding clusters) |
![]() |