超声共混合成Ni(HNCN)2/BiVO4复合可见光催化剂
张霞(), 宋扬, 王誉, 纪逯鹤, 杨媚, 孟皓
Ultrasonic Blending Synthesis of Ni(HNCN)2/BiVO4 Composite Visible-Light Induced Photocatalysts
ZHANG Xia(), SONG Yang, WANG Yu, JI Luhe, YANG Mei, MENG Hao

图3. Ni(HNCN)2/BiVO4复合颗粒的UV-Vis光谱和(Ahν)2随 (hν)变化曲线

Fig.3. UV-Vis diffuse reflectance spectra of Ni(HNCN)2/BiVO4 (a) and re-plotted curves of (Ahν)2vs (hν) for Ni(HNCN)2/BiVO4 composites (b) (h—Planck constant, A—absorbance, v—frequency)