[an error occurred while processing this directive]
超声共混合成Ni(HNCN)2/BiVO4复合可见光催化剂
张霞(), 宋扬, 王誉, 纪逯鹤, 杨媚, 孟皓
Ultrasonic Blending Synthesis of Ni(HNCN)2/BiVO4 Composite Visible-Light Induced Photocatalysts
ZHANG Xia(), SONG Yang, WANG Yu, JI Luhe, YANG Mei, MENG Hao

图1. Ni(HNCN)2、BiVO4 和Ni(HNCN)2/BiVO4复合颗粒的SEM像和EDS分析

Fig.1. SEM images (a~c, e, g) and EDS analyses (d, f, h) of Ni(HNCN)2 (a), BiVO4 (b), Ni(HNCN)2/BiVO4-0.3 (c, d), Ni(HNCN)2/BiVO4-2 (e, f), Ni(HNCN)2/BiVO4-3 (g, h) (The inset in Fig.1a is the particles observed under higher magnification)