2024铝合金表面PEDOT涂层的电化学制备及耐腐蚀性能
高博文1,2, 王美涵1(), 闫茂成2(), 赵洪涛2, 魏英华2, 雷浩2
Electrochemical Preparation and Corrosion Resistance of PEDOT Coatings on Surface of 2024 Aluminum Alloy
GAO Bowen1,2, WANG Meihan1(), YAN Maocheng2(), ZHAO Hongtao2, WEI Yinghua2, LEI Hao2

图4. 在DHS溶液(3.5 g/L (NH4)2SO2+0.5 g/L NaCl)中PEDOT/2024铝合金电极与2024铝合金电极偶接时的电位(E)和电流密度(i)

Fig.4. Galvanic potential and galvanic current density of the PEDOT/2024 aluminium electrode connected to the 2024 aluminium electrode in DHS solution (3.5 g/L (NH4)2SO2+0.5 g/L NaCl)