超高速激光熔覆镍基WC涂层的显微结构与耐磨性能 |
|||||||||||||||
| 张煜, 娄丽艳, 徐庆龙, 李岩, 李长久, 李成新 | |||||||||||||||
|
Microstructure and Wear Resistance of Ni-Based WC Coating by Ultra-High Speed Laser Cladding |
|||||||||||||||
| ZHANG Yu, LOU Liyan, XU Qinglong, LI Yan, LI Changjiu, LI Chengxin | |||||||||||||||
| 表1 超高速及低速激光熔覆实验参数 |
|||||||||||||||
| Table 1 Experimental parameters of ultra-high speed and conventional laser cladding |
|||||||||||||||
|
|||||||||||||||