超高速激光熔覆镍基WC涂层的显微结构与耐磨性能
|
|
Microstructure and Wear Resistance of Ni-Based WC Coating by Ultra-High Speed Laser Cladding
|
|
图7. No.1、No.2镍基WC涂层与45钢基体的摩擦系数和磨损失重 |
Fig.7. Friction coefficient and wear mass loss of No.1, No.2 Ni-based WC coatings and 45 steel substrate |
![]() |