超高速激光熔覆镍基WC涂层的显微结构与耐磨性能
|
|
Microstructure and Wear Resistance of Ni-Based WC Coating by Ultra-High Speed Laser Cladding
|
|
图4. No.1与No.2镍基WC涂层显微组织的SE和BSE像 |
Fig.4. Secondary electron (SE) (a, c) and BSE (b, d) images of the microstructure of No.1 (a, b) and No.2 (c, d) Ni-based WC coatings |
![]() |