超高速激光熔覆镍基WC涂层的显微结构与耐磨性能
|
|
Microstructure and Wear Resistance of Ni-Based WC Coating by Ultra-High Speed Laser Cladding
|
|
图3. No.1与No.2镍基WC涂层断面BSE像与过渡区元素EDS分析 |
Fig.3. BSE images (a, c) and corresponding EDS analyses of elements in transition zone (b, d) of No.1 (a, b) and No.2 (c, d) Ni-based WC coatings |
![]() |