Ti-B-N纳米复合涂层的设计、制备及性能
刘艳梅1, 王铁钢1(), 郭玉垚1, 柯培玲2, 蒙德强1, 张纪福1
Design, Preparation and Properties of Ti-B-N Nanocomposite Coatings
LIU Yanmei1, WANG Tiegang1(), GUO Yuyao1, KE Peiling2, MENG Deqiang1, ZHANG Jifu1

图9. 不同TiB2靶溅射功率沉积的Ti-B-N涂层磨痕形貌的OM像

Fig.9. OM images of worn scar of the Ti-B-N coatings prepared by different sputtering powers of the TiB2 target
(a) 0.8 kW (b) 1.2 kW (c) 1.6 kW (d) 2.0 kW (e) 2.4 kW